High Stability, High Efficiency & Long Service Life
As a screw barrel manufacturer in China, PIPLL supplies Single Screw Barrel units to extrusion plants in over 50 countries.
Developed by PIPLL, a screw barrel manufacturer focused on single screw extrusion components since 2002, our single screw and barrel adopts premium three-stage optimized structure and durable bimetallic alloy craftsmanship. Engineered for versatile plastic extrusion, PIPLL components deliver steady running performance and easy daily maintenance. It effectively boosts production efficiency and finished product quality, serving as an optimal core spare part for diverse single screw extrusion lines.
PIPLL Single Screw Barrel Application Scope
PIPLL Competitive Strengths
· Wide Compatibility
Fully interchangeable with Chinese and global single screw extruder brands globally, ready for direct installation.
Customized Solution
Tailor-made L/D ratio, compression ratio and mixing structure based on material property and output target.
Every PIPLL single screw barrel is built on one of three proven series. Each series shares the same 38CrMoAlA nitrided base material, the same optional bimetallic alloy layer, and the same three-stage screw profile — they differ in L/D ratio and maximum throughput, so you can match screw geometry to your output target instead of over-specifying the machine.
| Series | Screw diameter | L/D ratio | Max output | Typical application |
|---|---|---|---|---|
| Classic 33 | 45–150 mm | 33:1 | 150–1,500 kg/h | Standard PE, PP and PVC pipe, profile, sheet and pelletizing lines |
| High-Efficiency 38 | 45–150 mm | 38:1 | 150–2,000 kg/h | High-output film blowing, pipe, blow molding and recycling |
| High-Efficiency 40 | 75–120 mm | 40:1 | 700–2,000 kg/h | Premium throughput on large HDPE pipe and cast film lines |
Actual output depends on resin, die pressure, screw speed and line configuration, so the figures above are a starting point for sizing rather than a guarantee. Send us your existing screw drawing, barrel bore dimensions or machine nameplate and our engineers will confirm the closest series before quoting.
A single screw barrel is the heated cylindrical assembly that houses the rotating screw in a single screw extruder. The screw and barrel together convey solid resin, melt it by shear and conduction, homogenise the melt, and build the pressure needed to push polymer through the die. Geometry is divided into three zones along the screw length, and every zone is designed against a specific resin behaviour.
The feeding zone uses deep, constant-pitch flights to swallow cold granules or powder and move them forward without compacting too early. PIPLL applies a constant-pressure feed design together with grooved feed sections and forced cooling, which keeps the feed channel from slipping and makes output far less sensitive to die pressure. This is where unstable extrusion — surging, fluctuating output, inconsistent wall thickness — is usually born.
In the compression zone the flight depth reduces, squeezing the solid bed against the barrel wall so it melts through shear and conduction. The ratio of flight depth at the feed end to flight depth at the metering end is the compression ratio. A higher ratio generates more shear and better melt quality; a lower ratio reduces the risk of overheating and degradation. Unfilled polyolefins typically sit around 3:1 to 4:1, rigid PVC usually runs lower because of its narrow processing window, and heavily filled compounds need geometry that tolerates abrasion at high shear.
The metering zone has the shallowest, most uniform flight depth. Its job is to deliver a steady volumetric flow and enough pressure for the screen pack and die. Metering depth and length are matched to the target output and melt viscosity; too shallow and the screw starves, too deep and pressure control becomes unstable.
For demanding colour dispersion, filler loading or high-speed running, PIPLL adds a barrier section plus Maddock and pineapple mixing elements. The barrier flight separates already-melted polymer from the solid bed so unmelted granules cannot escape into the metering zone, while the Maddock and pineapple elements break up agglomerates and equalise melt temperature across the channel.
PIPLL manufactures to your drawing as well as to our own series. Both routes are quoted against the same inspection sheet, so a custom barrel and a catalogue barrel leave the factory held to identical tolerances.
| Parameter | Standard | Optional / note |
|---|---|---|
| Screw diameter | 45–150 mm | Outside this range quoted case by case |
| L/D ratio | 33:1 / 38:1 / 40:1 | Other ratios to drawing |
| Compression ratio | Set per resin | Confirm with the material data sheet |
| Base material | 38CrMoAlA | W6Mo5Cr4V2, D2 for high-wear duty |
| Surface treatment | Nitriding | Bimetallic alloy layer, HVOF tungsten carbide |
| Surface hardness | HRC 61 min. (bimetallic layer) | Nitrided layer approx. HV 900–1,000 (typical) |
| Nitriding depth | 0.4–0.7 mm (typical) | Deepened on request for abrasive duty |
| Surface roughness | Ra 0.4 µm | Finer finish for optical and medical grades |
| Screw straightness | ≤0.015 mm | Inspected per unit |
| Radial clearance | 0.10–0.25 mm (typical, size dependent) | Matched screw and barrel supplied as a pair |
| Feed section | Smooth bore | Grooved feed with forced cooling |
| Connection flange | Per drawing | Any bolt pattern, adapter plate supplied |
Most premature barrel failures are a material-selection problem, not a manufacturing problem. The table below maps the dominant wear mechanism of each resin family to the build PIPLL recommends in practice.
| Resin / compound | Dominant wear mechanism | Recommended build |
|---|---|---|
| PE, PP (unfilled) | Adhesive wear, moderate | Nitrided 38CrMoAlA |
| PE, PP with CaCO3, talc or glass fibre | Severe abrasion | Bimetallic alloy layer, HRC 61 min. |
| Rigid and plasticised PVC | Corrosion from HCl release plus abrasion | Bimetallic, high-chromium; corrosion resistance matters more than hardness |
| PET, PA (nylon) | Hydrolytic corrosion and abrasion | Bimetallic, corrosion-resistant grade; vented design recommended |
| PC, PMMA | Thermal, low abrasion | Nitrided, fine surface finish for optical clarity |
| ABS, PS | Moderate adhesive wear | Nitrided 38CrMoAlA |
| WPC, SPC | Severe abrasion from wood or mineral filler | Bimetallic or HVOF tungsten carbide |
| Post-consumer recycling | Mixed abrasion and corrosion, contamination | Bimetallic with wear allowance; matched to filtration stage |
| Food, medical, packaging | Corrosion, cleanability | Nitrided, Ra 0.4 µm or finer, no exposed coating defects |
| PVDF, TPE, silicone, rubber | Corrosion at low shear | Nitrided or special alloy; low-compression profile |
The choice is driven by material form, mixing requirement and output economics rather than by preference. As a screw barrel manufacturer we build both, so this comparison is deliberately practical.
| Criterion | Single screw barrel | Twin screw barrel |
|---|---|---|
| Material form | Pellets, regrind, powder with good bulk flow | PVC dry blend, powder, high filler loadings |
| Mixing and dispersion | Good with barrier and mixing elements | Excellent, intermeshing flights self-clean |
| Output per unit torque | Higher at low to medium output, lower energy per kg | Higher absolute output, needs more torque |
| Wear-part cost | One screw, one barrel — lowest replacement cost | Two screws, one barrel — higher replacement cost |
| Maintenance | Simple, in-house swap possible | Requires gearbox and flight-timing checks |
| Best fit | Pipe, profile, film, sheet, cable, blow molding, recycling | PVC dry blend, compounding, masterbatch, high-filler recipes |
If your line runs pelletised PE, PP, PS, ABS, PET or PA and your mixing requirement is met by a barrier screw with Maddock elements, a single screw barrel gives you the lowest cost per kilogram extruded and the cheapest wear-part replacement. It also retrofits easily: PIPLL barrels are interchangeable with most Chinese, European, American and Japanese single screw extruder brands, so a worn machine can be brought back to spec without changing the gearbox.
Powder blends, rigid PVC dry blend, masterbatch with high pigment loading and recipes above roughly 40 % filler usually justify a twin screw. In those cases the mixing and conveying job cannot be done reliably by a single flight. PIPLL supplies parallel twin screw barrels and conical twin screw barrels , and the selection logic is covered on those pages.
A single screw barrel is a wear part. Knowing which measurement actually indicates end of life prevents both premature replacement and the slow output loss that nobody notices until the line is 20 % down on rated capacity.
Measure radial clearance between flight OD and barrel bore with a feeler gauge or bore gauge at three points along the metering zone, rotated 120° apart, and record barrel bore roundness with an inside micrometer. Ultrasonic wall-thickness gauges are useful where an internal liner sleeve is fitted.
| Indicator | New condition | Service limit | Action |
|---|---|---|---|
| Radial clearance, flight to bore | 0.10–0.15 mm | 0.35 mm | Beyond 0.50 mm: replace or re-sleeve |
| Flight width loss | 0–1 mm | 3 mm | Beyond 4 mm: rebuild flights |
| Barrel bore ovality or taper | ≤0.05 mm | 0.15 mm | Rebore, hone or re-sleeve |
| Surface hardness | HV 900–1,000 (nitrided) | HV 700 | Re-nitriding rarely economical — replace |
Re-nitriding a worn screw is only worthwhile when the base geometry is still within tolerance and the hard layer has not been breached. Re-sleeving a barrel with an internal liner sleeve restores the bore at a fraction of new-barrel cost and is the usual route for large barrels. When clearance, hardness and bore geometry are all out of spec at once, a new matched screw and barrel set is the cheaper decision over a two-year horizon — and it removes the risk of a second failure mid-season.
PIPLL has manufactured extruder screws and barrels since 2002. Production runs from a 30,000 sq. ft facility on Jintang Island — China's largest screw barrel production cluster — with the export office in Ningbo, and every unit is quality-controlled in house rather than through subcontractors.
Base material is selected by duty: 38CrMoAlA for general nitrided barrels, W6Mo5Cr4V2 or D2 where abrasion is severe. Vacuum heat treatment stabilises the structure before machining so that dimensional change during nitriding stays predictable.
The process chain is raw material selection, vacuum heat treatment, CNC machining, deep-hole boring, then final grinding. Deep-hole boring is what determines bore straightness on long barrels; final grinding sets the Ra 0.4 µm finish and the ≤0.015 mm screw straightness that keep clearance stable over the service life.
Each batch is checked for dimensional accuracy, surface hardness and coating thickness before packing, and the inspection record is filed against the order so a replacement barrel can be reproduced from the same specification years later.
Single screw barrels are supplied from one set upward. Catalogue series typically ship within a few weeks of drawing confirmation; fully custom profiles take longer because the screw geometry is verified before machining. We export to Europe, the Americas, Southeast Asia and the Middle East, and can quote FOB or CIF against your forwarder.
A single screw barrel is the cylindrical, heated housing that contains one rotating screw in an extruder. It conveys plastic granules, melts them through shear and heat, mixes the melt, and holds the pressure needed to push polymer through the die.
A single screw barrel uses one flighted screw and suits pelletised resins such as PE, PP, PS, PET and PA. A twin screw barrel uses two intermeshing screws and handles powder blends, rigid PVC dry blend and high filler loadings with better mixing and self-cleaning.
33:1 is the standard choice for pipe, profile and general extrusion. 38:1 gives better melting and mixing at higher output and suits film, blow molding and recycling. 40:1 is for premium throughput on large lines where melt homogeneity has to hold at high screw speed.
Compression ratio is the flight depth at the feed zone divided by the flight depth at the metering zone. Unfilled polyolefins typically run at about 3:1 to 4:1, rigid PVC lower because of its narrow processing window, and filled compounds are set with both abrasion and shear heat in mind.
PIPLL single screw barrels use 38CrMoAlA nitrided steel as standard, with W6Mo5Cr4V2 or D2 for high-wear duty. A reinforced bimetallic alloy layer with HRC 61 minimum is available, as is HVOF tungsten carbide coating for severely abrasive compounds.
The reliable signs are falling output at constant screw speed, rising melt temperature, growing radial clearance between flight and bore, and visible wear steps on the flight lands. Measuring clearance at three points along the metering zone is the quickest confirmation.
Yes. Send the screw drawing, barrel bore dimensions or the machine nameplate and PIPLL will reproduce the geometry, including flange pattern and feed section, so the barrel installs without modifying the gearbox or hopper.
Yes, and we recommend it. A new screw in a worn barrel loses output almost immediately because clearance is already open, so matched sets are quoted together and inspected as a pair.
The minimum order is one set. Catalogue series normally ship within a few weeks of drawing confirmation, while fully custom screw profiles take longer because geometry is verified before machining. Exact dates are confirmed with the quotation.
Often yes. Re-sleeving with an internal liner sleeve or re-boring and honing restores the bore when the barrel body is still sound. Replacement is the better decision when hardness, bore geometry and clearance are all out of specification.
PIPLL single screw barrels are built to be interchangeable with common single screw extruder brands worldwide, including Chinese, European, American and Japanese machines, and are supplied ready for direct installation.
PE, PP, PVC, PET, PS, ABS, PC, PMMA, PA, PVDF, EVA, PLA, WPC, SPC, TPE, silicone and rubber, across pipe, profile, film blowing, cast film, sheet, blow molding, foaming, cable, chemical fibre, recycling and pelletizing.
Send us your screw drawing, barrel dimensions or process details — resin, target output, screw diameter and existing machine — and PIPLL will confirm the series, material build and lead time. Quotes are usually returned within one working day.
Barrier screw with grooved feed and forced cooling, up to 2,000 kg/h at L/D 33:1, 38:1 or 40:1.


+86 15267878906