Through Hardened Screw
  • Through Hardened Screw
  • Through Hardened Screw

Through Hardened Screw

  • PIPLL utilizes premium imported and domestic specialty steels—including the PIPLL-QY1 through PIPLL-QY8 series. Through rigorous quenching and annealing treatments, these screws achieve an optimal balance of high hardness and toughness, making them ideal for processing high-wear materials.

    Advantages

    High toughness and hardness with high temperature resistance and corrosion resistance, which can greatly meet the high qualified rate of customers' final products.

    Application

    General plastics & engineering plastics with below 70% glass fiber filling.

  • Through Hardened Screw Material Parameters

    PIPLL-QY1 Through Hardened Screw

    Parameter

    Details

    Material Name

    PIPLL-QY1

    Main Components

    C, Cr, V, Mo, Mn

    Hardness Range

    56-60HRC

    Performance

    Wear resistance

    Applicable Plastics

    General plastics, PA, LCP, PBT, POM with glass fiber less than 30% and transparent PC.


  • PIPLL-QY2 Through Hardened Screw

    Parameter

    Details

    Material Name

    PIPLL-QY2

    Main Components

    C, W, Mo, Cr, V

    Hardness Range

    60-65HRC

    Performance

    Super wear resistance

    Applicable Plastics

    General plastics, PA, LCP, PBT, POM, PPSU, PEEK, PEI, etc. with glass fiber less than 50%.


  • PIPLL-QY3 Through Hardened Screw

    Parameter

    Details

    Material Name

    PIPLL-QY3

    Main Components

    C, Cr, Mo, Mn, V

    Hardness Range

    58-62HRC

    Performance

    High wear resistance

    Applicable Plastics

    General plastics and engineering plastics, PA, LCP, PBT, POM, PPSU, PEI with glass fiber less than 40% and transparent PC.


  • PIPLL-QY4 Through Hardened Screw

    Parameter

    Details

    Material Name

    PIPLL-QY4

    Main Components

    C, W, Mo, Cr, V

    Hardness Range

    62-65HRC

    Performance

    Super wear resistance, corrosion resistance

    Applicable Plastics

    General plastics and engineering plastics, PA, LCP, PBT, POM, PPSU, PEEK, PEI with glass fiber less than 50% and other special plastics.


  • PIPLL-QY6 Through Hardened Screw

    Parameter

    Details

    Material Name

    PIPLL-QY6

    Main Components

    C, W, Mo, Cr, V

    Hardness Range

    62-65HRC

    Performance

    Ultra high wear resistance and corrosion resistance

    Applicable Plastics

    PEP, PEP, POP, etc. With less than 70% glass fiber.


  • PIPLL-QY7 Through Hardened Screw

    Parameter

    Details

    Material Name

    PIPLL-QY7

    Main Components

    C, Cr, Mn, V

    Hardness Range

    50-56HRC

    Performance

    Wear resistance, high corrosion resistance

    Applicable Plastics

    Mainly applicable to optical products requiring high finish and strong corrosion resistance.


  • PIPLL-QY8 Through Hardened Screw

    Parameter

    Details

    Material Name

    PIPLL-QY8

    Main Components

    C, Ni, Co, Cr

    Hardness Range

    56-58HRC

    Performance

    wear resistance, corrosion resistance

    Applicable Plastics

    Suitable for high-temperature plastics with molding temperature higher than 300℃.(not applicable to plastics with low molding temperature).


  • Halogen Free Special Screw

    Parameter

    Details

    Material Name

    Halogen Free Screw

    Main Components

    W, Cr, Ni

    Hardness Range

    62-67HRC

    Performance

    ultra-high wear resistance, ultra-high corrosion resistance

    Applicable Plastics

    To special high glass fiber and ultra halogen-free plastics, such as PA46, PA4T, PA9T, PSM, DSM and other high acid and strong corrosion engineering plastics.