Bimetallic Extrusion Barrel
  • Bimetallic Extrusion Barrel
  • Bimetallic Extrusion Barrel
  • Bimetallic Extrusion Barrel
  • Bimetallic Extrusion Barrel
  • Bimetallic Extrusion Barrel
  • Bimetallic Extrusion Barrel
  • Bimetallic Extrusion Barrel

Bimetallic Extrusion Barrel

  • PIPLL Bimetallic Barrels: Tough, Durable, Efficiency-Driven

    PIPLL specializes in high-quality bimetallic barrel manufacturing—built for the harshest industrial demands. Delivering top-tier wear resistance and rock-solid durability, PIPLL ensure stable, efficient performance in every operation.

    Using advanced metallurgical technology, PIPLL precisely fuse dual metals to create barrels that withstand high temperatures and pressures, while maximizing service life and performance. PIPLL combines innovation and precision to be your trusted industry partner, helping you cut costs, boost efficiency, and lead in production capability.

    Choose PIPLL bimetallic barrels—choose quality, choose unwavering reliability!

  • Technical Specifications

     

    PIPLL Bimetallic Barrels

    Item

    PIPLL01 Alloy

    PIPLL02 Alloy

    PIPLL03 Alloy

    PIPLL04 Alloy

    Alloy Components

    Fe+Ni+Cr+B<br>(Fe:65, Ni:14, Cr:8, B:3.5)

    Ni+Cr+Co+B

    Ni+Cr+Co+V+B

    Ni+Wc+Cr+B<br>(Ni:50, Wc:1535, Cr:68, B:2.5~3.2)

    Wear Resistance

    ★★★ Very Good

    ★★ Good

    ★★★ Very Good

    ★★★★ Excellent

    Corrosion Resistance

    ★★ Good

    ★★★ Very Good

    ★★★ Very Good

    ★★★ Very Good

    Alloy Thickness

    2~3mm

    1.5~2mm

    1.5~2mm

    1.5~2mm

    Hardness

    HRC 58-65

    HRC 50-58

    HRC 55-60

    HRC 55-65

    Max Working Temperature

    ≤400℃

    ≤450℃

    ≤450℃

    ≤600℃

    Thermal Expansion Coefficient (RT~250℃)

    11.4x10⁻⁶/℃

    11.0x10⁻⁶/℃

    11.0x10⁻⁶/℃

    11.5x10⁻⁶/℃

    Thermal Expansion Coefficient (RT~400℃)

    11.4x10⁻⁶/℃

    11.4x10⁻⁶/℃

    12.4x10⁻⁶/℃

    12x10⁻⁶/℃

    Workable Length Range

    700mm~3000mm per piece

    Commonly Used Base Steel

    40Cr, 42CrMo

    Rating Standard: ★★★★ Excellent; ★★★ Very Good; ★★ Good

     